Deloro® alloy N-6 PM, P/M, tested at 538°C (1000°F)
  Subcategory: Superalloy; Nickel Base 
Material Notes:  Nickel content as balance. Adhesive wear test data: P/M 0.1, cast 0.1; Abrasive wear test data: P/M 17, cast 35. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wear parts.  Data provided by the manufacturer, Deloro Stellite Inc. 
  
  
    | Available Properties | 
   
    
    - Density
 
- Hardness, Brinell
 
- Hardness, Knoop
 
- Hardness, Rockwell A
 
- Hardness, Rockwell B
 
- Hardness, Rockwell C
 
- Hardness, Vickers
 
- Tensile Strength, Ultimate
 
- Elongation at Break
 
- Modulus of Elasticity
 
 
   |   
   |   
 | 
   | 
  
  