ECOMold® 135 Copper Mold Material
Subcategory: Copper Alloy; Nonferrous Metal
Material Notes: ECOMold® copper alloys (beryllium-free) are engineered specifically for plastics industry applications. ECOMold® 135 has superior thermal conductivity compared to other common mold materials. This mold material has proven to be highly effective for injection molding, blow molding, thermoforming, and other plastic processing applications. ECOMold® 95 is used in applications requiring a high thermal conductivity level such as cores, core inserts, cavities - inserts, core pins, blow pins, ejector pins, lifters, sleeves, and sprue bushings. Information provided by ECOMold.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Strength
- Charpy Impact
- Electrical Resistivity
- CTE, linear 68°F
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|