Elkem Gransil® 5-25 mm Granulated Ferrosilicon
Subcategory: Metal
Material Notes:
Ferrosilicon is used both as a deoxidizer after decarburization –because of the strong affinity for oxygen of silicon– and for alloying. Silicon increases namely strength and wear resistance, elasticity (spring steels), scale resistance (heat resistant steels), and lowers electrical conductivity and magnetostriction (electrical steels).
| Available Properties |
- Density
- Bulk Density
- Particle Size
- Abrasion
- Heat of Fusion
- Specific Heat Capacity
- Melt Temperature
- Angle of Repose
- Solubility in alkalis
- Solubility in Fluorhydric acid
- Solubility in Mineral Acids
- Solubility in Water %
|
|
|
|
| Property Data |