Elkem Low Al Ferrosilicon FeSi 0.10 Al
Subcategory: Metal
Material Notes: Low Al Ferrosilicon compared to regular ferrosilicon will lower the content of aluminum inclusions in the final steel. In high carbon steels use of low Al FeSi will assist in the prevention of nozzle blockage during continuous casting. Reduced amounts of aluminum inclusions will help to avoid surface defects, particularly relevant to mirror finish stainless steel. For the production of tyre cord, in which inclusion control is also important, we recommend the use of our range of High Purity Ferrosilicon.
| Available Properties |
- Density
- Bulk Density
- Particle Size
- Heat of Fusion
- Specific Heat Capacity
- Melt Temperature
- Angle of Repose
- Solubility in alkalis
- Solubility in Fluorhydric acid
- Solubility in Mineral Acids
- Solubility in Water %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|