Elkem Low Carbon Ferrosilicon LC FeSi 65
Subcategory: Metal
Material Notes: This product is added as a deoxidant and as an alloying element to steels that require a special low carbon content, e.g. non-grain oriented electrical steels. Low Carbon FeSi 65 lowers the electrical conductivity and magnetostriction of electrical steels. When FeSi 75% dissolves in steel, it increases the temperature of the bath while FeSi 65% is almost temperature neutral,
| Available Properties |
- Density
- Bulk Density
- Particle Size
- Heat of Fusion
- Specific Heat Capacity
- Melt Temperature
- Angle of Repose
- Solubility in alkalis
- Solubility in Fluorhydric acid
- Solubility in Mineral Acids
- Solubility in Water %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|