Havar® High-Strength Non-Magnetic Cobalt-Base Alloy
Subcategory: Nonferrous Metal; Cobalt Alloy
Material Notes: Co42.5/Cr20/Ni13/Fe/W/Mo/Mn Information provided by Goodfellow.
| Available Properties |
- Density
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|