Goodfellow Iron 40/Nickel 38/Boron 18 Alloy
Subcategory: Iron Base; Solder/Braze Alloy; Metal
Material Notes: General Description:Metallic glass (glassy alloy) or amorphous metal. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers. Information provided by Goodfellow.
| Available Properties |
- Density
- Vickers Microhardness
- Tensile Strength at Break
- Tensile Modulus
- Electrical Resistivity
- Magnetic Coercive Force, Hc
- Magnetic Saturation Flux Density, Bmax
- Magnetic Remanence, Br
- Curie Temperature
- Crystallization Temperature
- Maximum Service Temperature, Air
- Saturation magnetostriction (x10^-6)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|