Goodfellow Magnetic Shielding Alloy - Nickel Base
Subcategory: Electronic/Magnetic Alloy; Nickel Alloy; Nonferrous Metal
Material Notes: General Description:High Nickel magnetically soft alloy used for magnetic shielding, high quality but low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head laminations and magnetometer bobbin cores. Information provided by Goodfellow.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength at Break
- Tensile Modulus
- Izod Impact, Unnotched
- Electrical Resistivity
- Magnetic Permeability
- Magnetic Coercive Force, Hc
- Magnetic Remanence, Br
- Curie Temperature
- CTE, linear 20°C
- Thermal Conductivity
- Saturation Induction (T)
|
|
|
|