Nichrome®, Tophet A® Nickel 80 Chromium 20 Alloy
Subcategory: Nickel Alloy; Nonferrous Metal
Material Notes: Information provided by Goodfellow.
| Available Properties |
- Density
- Tensile Strength at Break
- Elongation at Break
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
|
|
|
|