Goodfellow T1-Thermocouple Alloy
Subcategory: Electronic/Magnetic Alloy; Nickel Alloy; Nonferrous Metal
Material Notes: General DescriptionThe positive element of the type K thermocouple alloy the negative being T2. The thermocouple can be used up to 1250C in oxidizing atmospheres and is the probably the most common in use. It is also the positive element of the type E thermocouple with Constantan as the negative; the thermoelectric power of type E thermocouples is the highest amongst all standard couples Information provided by Goodfellow.
| Available Properties |
- Density
- Tensile Strength at Break
- Elongation at Break
- Modulus of Elasticity
- Izod Impact, Unnotched
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 1000°C
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|