Goodfellow T2-Thermocouple Alloy
Subcategory: Electronic/Magnetic Alloy; Nickel Alloy; Nonferrous Metal
Close Analogs: Composition Notes: Al + Mn + Si content 5 wt%.
Material Notes: General DescriptionThe negative element of the type K thermocouple, the positive being T1. The thermocouple can be used up to 1250C in oxidizing atmospheres, and probably is the most common in use. Information provided by Goodfellow.
| Available Properties |
- Density
- Tensile Strength at Break
- Elongation at Break
- Izod Impact, Unnotched
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 1000°C
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |