Haynes® 718 alloy, cold rolled, solution-treated and aged sheet, tested at 760°C (1400°F)
Subcategory: Superalloy; Nickel Base
Key Words: UNS N07718, AMS 5596, AMS 5597, AMS 5662, AMS 5664, AMS 5832, AMS 5589, AMS 5590, NACE MR-01-75, ASTM B626
Material Notes: Nickel content to balance. Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications include a variety of fabricated component applications in both aircraft and land-based turbine engines including rings, casings, and many types of formed sheet metal components; also used for fasteners and instrumentation parts, also various applications for oil/gas well down hole and well head components. Data provided by the manufacturer, Haynes International, Inc.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|