Haynes® 718 alloy, cold rolled, solution-treated and aged sheet, tested at 870°C (1600°F)

 

Subcategory: Superalloy; Nickel Base

Key Words: UNS N07718, AMS 5596, AMS 5597, AMS 5662, AMS 5664, AMS 5832, AMS 5589, AMS 5590, NACE MR-01-75, ASTM B626

Material Notes:
Nickel content to balance. Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications include a variety of fabricated component applications in both aircraft and land-based turbine engines including rings, casings, and many types of formed sheet metal components; also used for fasteners and instrumentation parts, also various applications for oil/gas well down hole and well head components.

Data provided by the manufacturer, Haynes International, Inc.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Modulus of Elasticity at Elevated Temperature
  • Electrical Resistivity
  • Electrical Resistivity at Elevated Temperature
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。