Haynes® Hastelloy® X alloy, sheet, tested at RT
Subcategory: Superalloy; Nickel Base
Key Words: AMS 5798, AMS 5799, AMS 5888, UNS N06002, AMS 5536, AMS 5588, AMS 5754
Material Notes: Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications include materials for fabricated or forged parts in gas turbine engines, and chemical and petrochemical plants, power plant and industrial heating applications. Data provided by the manufacturer, Haynes International, Inc.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- CTE, linear 500°C
- CTE, linear 1000°C
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|