Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated, tested at 760°C (1400°F)
Subcategory: Superalloy; Nickel Base
Key Words: ASME SB-622, ASME SB-626 ASTM B-574, ASTM B-575, ASTM B-619, ASTM B-622, ASTM B-626, DIN 17744 No. 2.4602, TUV Werstoffblatt 479, UNS N06022, ASME SB-574, ASME SB-575, ASME SB-619, NACE MR-01-75
Material Notes: Outstanding resistance to localized corrosion and excellent resistance to stress corrosion cracking, best alloy to use as a universal weld filler metal to resist corrosion of weldments. Applications include acetic acid/acetic anhydride, acid etching, cellophane manufacturing, chlorination systems, complex acid mixtures, electro-galvanizing rolls, expansion bellows, flue gas scrubber systems, geothermal wells, HF furnace scrubbers, incinerator scrubber systems, nuclear fuel reprocessing, pesticide production, phosphoric acid production, pickling systems, plate heat exchangers, selective leaching systems, SO2 cooling towers, sulfonation systems, tubular heat exchangers, weld overlay-valves. Data provided by the manufacturer, Haynes International, Inc.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Charpy Impact
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|