Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), notched

 

Subcategory: Superalloy; Nickel Base

Key Words: ASME SB-622, ASME SB-626 ASTM B-574, ASTM B-575, ASTM B-619, ASTM B-622, ASTM B-626, DIN 17744 No. 2.4602, TUV Werstoffblatt 479, UNS N06022, ASME SB-574, ASME SB-575, ASME SB-619, NACE MR-01-75

Material Notes:
Outstanding resistance to localized corrosion and excellent resistance to stress corrosion cracking, best alloy to use as a universal weld filler metal to resist corrosion of weldments. Applications include acetic acid/acetic anhydride, acid etching, cellophane manufacturing, chlorination systems, complex acid mixtures, electro-galvanizing rolls, expansion bellows, flue gas scrubber systems, geothermal wells, HF furnace scrubbers, incinerator scrubber systems, nuclear fuel reprocessing, pesticide production, phosphoric acid production, pickling systems, plate heat exchangers, selective leaching systems, SO2 cooling towers, sulfonation systems, tubular heat exchangers, weld overlay-valves.

Data provided by the manufacturer, Haynes International, Inc.

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Modulus of Elasticity
  • Modulus of Elasticity at Elevated Temperature
  • Charpy Impact
  • Electrical Resistivity
  • Electrical Resistivity at Elevated Temperature
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Specific Heat Capacity
  • Specific Heat Capacity at Elevated Temperature
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。