Hastelloy® C-4 alloy, 12.7 mm (1/2 in.) thick plate, heat treated at 1066°C, rapid quenched, tested at 538°C (1000°F)
Subcategory: Superalloy; Nickel Base
Key Words: ASME SB-622, ASME SB-626, UNS N06455, ASME SB-574, ASME SB-575, ASME SB-619, nickel alloy
Material Notes: Nickel content to balance. High temperature stability even after aging in the 650-1040°C (1200-1900°F) range as evidenced by good ductility and corrosion resistance. Resists the formation of grain-boundary precipitates and is therefore suitable for use in most chemical process applications in the as-welded condition. C-4 resists stress-corrosion cracking and oxidizing atmospheres up to 1040°C (1900°F). It has exceptional resistance to hot contaminated mineral acids, solvents, chlorine and chlorine-contaminated media (organic and inorganic), dry chlorine, formic and acetic acids, acetic anhydride, seawater and brine solutions. Data provided by the manufacturer, Haynes International, Inc.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|