Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld 3.2 mm diameter filler wire, tested at 760°C (1400°F)
Subcategory: Superalloy; Nickel Base
Key Words: ASME SB622, ASME SB626, ASME SB366, UNS N06030, ASME SB581, ASME SB582, ASME SB619
Material Notes: Nickel content to balance. Cb and Ta content = 0.3-1.5%. Superior corrosion resistance to commercial phosphoric acids and oxidizing acid mixtures. Typical applications include phosphoric acid service, sulfuric acid service, nitric acid service, nuclear fuel reprocessing, nuclear waste processing, pickling operations, petrochemicals, fertilizer manufacture, pesticide manufacture, and gold ore extraction. Data provided by the manufacturer, Haynes International, Inc.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Charpy Impact
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 250°C
- CTE, linear 500°C
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|