Hogen Duralloy H20TC, 70 Tungsten Carbide/30 Copper PM Metal Composite
Subcategory: Metal Matrix Composite; Copper Alloy; Tungsten Alloy; Nonferrous Metal
Key Words: Hogen Industries Powder Metallurgy Metal Composite; Copper Alloys
Material Notes: Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver. Typical Resistance Welding Applications: Extremely hard and wear resistant to meet the more demanding requirements of electrical upsetting and electro-forging. Data provided by Hogen Industries.
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Electrical Resistivity
|
|
|
|
| Property Data |