Hogen Diemitech™ Tungsten-Based Metal

 

Subcategory: Tungsten Alloy; Nonferrous Metal; Refractory Metal

Key Words: Hogen Industries Tungsten Alloys

Material Notes:
Diemitech is a new tungsten-based material used for high temperature tooling, die casting, extrusion dies, hot upsetting, and electro brazing. It has a higher tungsten content than similar available materials, giving it superior refractory properties resulting in greater resistance to erosion and wear. Diemitech maintains good thermal conductivity and physical properties at high working temperatures.

Advantages of using Diemitech:Tools run much cooler because its thermal conductivity is 3-4 times that of steel.
Low thermal expansion - 1/3 that of steel.
Withstands thermal shock.
Excellent mechanical properties at elevated temperatures.
Resists erosion and scaling.
Minimizes soldering and heat checking.
No costly treatment required, normally can be placed into service as machines.
Superior physical properties compared to steel at high working temperatures.
Diemitech is machinable, similar to cast iron.

Data provided by Hogen Industries.

Available Properties
  • Density
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。