Haynes® R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F), tested at 760°C (1400°F)
Subcategory: Superalloy; Nickel Base
Key Words: UNS N07041, AMS 5545, AMS 5712
Material Notes: Nickel content as balance. Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications include afterburner parts and nozzle diaphragm partitions in current gas turbine engines. Formed with success on drop-hammers, expanding mandrels and stretch formers. Data provided by the manufacturer, Haynes International, Inc.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Poissons Ratio
- Poissons Ratio at Elevated Temperature
- Shear Modulus
- Shear Modulus at Elevated Temperature
- Magnetic Permeability
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|