Haynes® Waspaloy™ alloy, sheet, tested at 980°C (1800°F)
Subcategory: Superalloy; Nickel Base
Key Words: AMS 5544
Material Notes: Nickel content to balance. Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, good resistance to gas turbine combustion gas environments at temperatures up to 870°C (1600°F). Widely used as a wrought material for forged and fabricated gas turbine and aerospace components. Data provided by the manufacturer, Haynes International, Inc.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- CTE, linear 500°C
- CTE, linear 1000°C
- Thermal Conductivity at Elevated Temperature
- Melting Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|