Special Metals Nickel 200
Subcategory: Pure Element; Nickel Alloy; Nonferrous Metal
Key Words: ASME SB-160 - SB-163, Boiler Code Sections III, VIII, IX; DIN 17740, 17750-17754, Nickel, Ni, UNS N02200; BS 3072-3076 (NA11); ASTM B 160 - B 163, B 725, B 730, Werkstoff Nr. 2.4060, 2.4066
Material Notes: Nickel content above includes cobalt. Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Used for a variety of processing equipment, particularly to maintain product purity in handling foods, synthetic fibers, and alkalis. Standard product forms are round, flats, pipe, tube, plate, sheet, forging stock, strip, and wire. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Electrical Resistivity
- Curie Temperature
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|