Special Metals Nickel 222
Subcategory: Pure Element; Nickel Alloy; Nonferrous Metal
Key Words: ASTM F 239; BS 3504; DIN 17740; Werkstoff Nr. 2.4053, Nickel, Ni
Material Notes: Nickel content above includes cobalt. Wrought nickel with an addition of magnesium for electronic applications. The magnesium provides activation for cathodes of thermionic devices. Used for sleeves of indirectly heated oxide-coated cathodes. Ferromagnetic. Standard product forms are strip, tube, and wire. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|