Special Metals MONEL™ Alloy 400
Subcategory: Superalloy; Copper Alloy; Nickel Alloy
Key Words: AFNOR NU30; SAE AMS 4544, 4574, 4575, 4675, 4730, 4731, 7233; DIN 17743, 17750 - 17754, ASME SB-127, SB-163 - SB-165, SB-564, Boiler Code Sections III, IV, VIII, IX; AECMA Pr EN 2305, Monel Nickel-Copper Alloy, UNS N04400; BS 3072-3076 (NA 13); ASTM B 127, B 163 - B 165, B 564, Werkstoff Nr. 2.4360, 2.4361; VdTUV 263; MIL-T-1368, MIL-T-23520, MIL-N-24106; QQ-N-281; NACE MR-01-75
Material Notes: Nickel content above includes cobalt. A nickel-copper alloy with high strength and excellent corrosion resistance in a range of media including sea water, hydrofluoric acid, sulfuric acid, and alkalis. Used for marine engineering, chemical and hydrocarbon processing equipment, valves, pumps, shafts, fittings, fasteners, and heat exchangers. Standard product forms are round, hexagon, flats, forging stock, pipe, tube, plate, sheet, strip, and wire. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Electrical Resistivity
- Curie Temperature
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|