Special Metals MONEL™ Alloy K-500
Subcategory: Superalloy; Copper Alloy; Nickel Alloy
Key Words: DIN 17743, 17752, 17754; Werkstoff Nr. 2.4375; QQ-N-286; NACE MR -01-75, Monel Nickel-Copper Alloy, UNS N05500; BS 3072 - 3076 (NA18); ASME Boiler Code Section VIII; SAE AMS 4676; MIL-N-24549
Material Notes: A precipitation-hardenable nickel-copper alloy that combines the corrosion resistance of MONEL alloy 400 with greater strength and hardness. It also has low permeability and is nonmagnetic to under -150°F (-101°C). Used for pump shafts, oil-well tools and instruments, doctor blades and scrapers, springs, valve trim, fasteners, and marine propeller shafts. Standard product forms are round, hexagon, flats, forging stock, pipe, tube, plate, sheet, strip, and wire. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Electrical Resistivity
- Magnetic Permeability
- Curie Temperature
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|