Special Metals INCONEL® Alloy 600
Subcategory: Superalloy; Nickel Base
Key Words: Inconel 600, ASTM B163, ASTM B166, ASTM B167, ASTM B168, ASTM B366, ASTM B516, ASTM B517, ASTM B564, ASTM B751, ASME SB-163, SB-166 - SB-168, SB-564, Boiler Code Sections I, III, VIII, IX, Nickel-Chromium Alloy, NACE MR-01-75; QQ-W-390; MIL-R-5031, MIL-T-23227, MIL-N-23228, MIL-N-23229; AFNOR NC 15 Fe, SAE AMS 5540, 5580, 5665, 5687, 7232; DIN 17742, 17750 - 17754; Werkstoff Nr. 2.4816; VdTUV 305, UNS N06600; BS 3072 - 3076 (NA14)
Material Notes: Nickel content above includes cobalt. A nickel-chromium alloy with good oxidation resistance at high temperatures and resistance to chloride-ion stress-corrosion cracking, corrosion by high-purity water, and caustic corrosion. Used for furnace components, in chemical and food processing, in nuclear engineering, and for sparking electrodes. Standard product forms are round, hexagon, extruded section, flats, forging stock, pipe, tube, plate, sheet, strip, and wire. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Electrical Resistivity
- Magnetic Permeability
- Curie Temperature
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|