Special Metals INCONEL® Alloy C-276
Subcategory: Superalloy; Nickel Base
Key Words: ASME SB-574, SB-575, SB-619, SB-622, SB-626, Boiler Code Sections I, III, VIII, IX; Werkstoff Nr. 2.4819, Nickel-Chromium Alloy; UNS N10276; ASTM B 574, B 575, B 619, B 622, B 626, B 751; NACE MR-01-75; DIN 17744, 17750-17752
Material Notes: Nickel content as remainder. A nickel-molybdenum-chromium alloy with an addition of tungsten having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially resistant to pitting and crevice corrosion. The low carbon content minimizes carbide precipitation during welding to maintain corrosion resistance in as-welded structures. Used in pollution control, chemical processing, pulp and paper production, and waste treatment. Standard product forms are round, forging stock, tube, pipe, plate, sheet, strip, and wire. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|