Special Metals INCONEL® Alloy HX
Subcategory: Superalloy; Nickel Base
Key Words: ASME SB-435, SB-572, SB-619, SB-622, SB-626, Boiler Code Sections III, VIII, IX, Nickel-Chromium Alloy; Werkstoff Nr. 2.4665, SAE AMS 5536, 5587, 5588, 5754, 5798, 7237; WL Nr. 2.4665; AFNOR NC 22 Fe D; NACE MR-01-75; AECMA Pr EN 2182 - 2185, UNS N06002; BS HR6, HR204; ASTM B 435, B 572, B 619, B 622, B 626, B 751
Material Notes: Nickel content as remainder. A nickel-chromium-iron-molybdenum alloy with outstanding strength and oxidation resistance at temperatures to 2200°F (1200°C). Matrix stiffening provided by the molybdenum content results in high strength in a solid-solution alloy having good fabrication characteristics. Used in gas turbines, industrial furnaces, heat-treating equipment, and nuclear engineering. Standard product forms are round, extruded section, flats, forging stock, plate, sheet, strip, and wire. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|