Special Metals NIMONIC™ Alloy 75
Subcategory: Superalloy; Nickel Base
Key Words: Nickel-Chromium Alloy; UNS N06075; BS HR5, HR203, HR403, HR504; DIN 17742, 17750 - 17752; Werkstoff Nr. 2.4951, 2.4630, WL Nr. 2.4630; AFNOR NC 20T; AECMA Pr EN 2293, 2294, 2302, 2306-2308, 2402, 2411
Material Notes: Nickel content as remainder. A nickel-chromium alloy with good mechanical properties and oxidation resistance at high temperatures. Used for sheet-metal fabrications in gas-turbine engines, for components of industrial furnaces, for heat-treating equipment and fixtures, and in nuclear engineering. Standard product forms are round, hexagon, flats, extruded section, tube, pipe, plate, sheet, strip, and wire. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|