Special Metals NIMONIC™ Alloy 105
Subcategory: Superalloy; Nickel Base
Key Words: BS HR3; Werkstoff Nr. 2.4634; AFNOR NK 20 CDA; AECMA Pr EN 2179-2181, WL Nr. 2.4634, Nickel-Chromium Alloy
Material Notes: Nickel content as remainder. A precipitation-hardenable nickel-cobalt-chromium alloy with an addition of molybdenum for solid-solution strengthening. The relatively high aluminum content enhances both strength (through greater precipitation hardening) and oxidation resistance. The alloy has high creep-rupture properties at temperatures to about 1740°F (950°C). Used in gas turbines for blades, discs, and shafts. Standard product forms are round and extruded section. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|