Special Metals NIMONIC™ Alloy PE11
Subcategory: Superalloy; Nickel Base
Key Words: Nickel-Chromium Alloy; DTD 5037; AFNOR Z8 NC D38
Material Notes: Iron content as remainder. A nickel-iron-chromium alloy precipitation hardened by titanium and aluminum and solid-solution strengthened by an addition of molybdenum. It was developed as a high-strength sheet alloy for use at temperatures to 1020°F (550°C). The high iron content provides good workability and also relatively high tensile ductility, especially after welding. Used for components of gas turbines. Standard product forms are round, flats, extruded section, plate, sheet, and wire. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Magnetic Permeability
- Specific Heat Capacity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|