Special Metals NIMONIC™ Alloy AP1
Subcategory: Superalloy; Nickel Base
Key Words: Nickel-Chromium Alloy
Material Notes: A nickel-cobalt-chromium alloy produced by powder metallurgy. It is strengthened by precipitation hardening and by solid-solution strengthening through a molybdenum addition. Production of the alloy involves compaction, by hot isostatic pressing, of pre-alloyed powder made by argon gas atomization. The process yields an alloy with outstanding strength properties and forgeability. Used for discs in gas turbines. The standard product form is round. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- CTE, linear 20°C
- Specific Heat Capacity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|