Special Metals INCOLOY® Alloy 800HT™
Subcategory: Superalloy; Iron Base
Key Words: ASME SB-163, SB-407 - SB-409, SB-564, Boiler Code Sections I, VIII, UNS N08811; ASTM B 163, B 407 - B 409, B 514, B 515, B 564; BS 3072, 3074, 3076 (NA15H), Werkstoff Nr. 1.4876; S.E.W. 470
Material Notes: A nickel-iron-chromium alloy having the same basic composition as INCOLOY alloy 800 but with significantly higher creep-rupture strength. The higher strength results from close control of the carbon, aluminum, and titanium contents in conjunction with a high-temperature anneal. Used in chemical and petrochemical processing, in power plants for super-heater and reheater tubing, in industrial furnaces, and for heat-treating equipment. Standard product forms are round, flats, forging stock, pipe, tube, plate, sheet, strip, and wire. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Electrical Resistivity
- Magnetic Permeability
- Curie Temperature
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|