Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 30% Cold Work
Subcategory: Superalloy; Nickel Base
Material Notes: Niobium content in composition table also include tantalum Tensile strength (ultimate and yield), elongation, and reduction of area values are for annealed then cold worked samples. This produces ASTM grain size 10.0. Other property values are typical of this alloy. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|