Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 3.50 inch (88.9 mm) o.d. and 0.219 inch (5.49 mm) Thickness
Subcategory: Superalloy; Nickel Base
Material Notes: Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co. Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Drawn Tube, 3.50 inch (88.9 mm) o.d. and 0.219 inch (5.49 mm) Thickness. Other property values are typical of INCONEL® alloy 690. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|