Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, 3 Part Heat Treatment, 0.062 inch (1.57 mm) Thickness
Subcategory: Superalloy; Iron Base; Nickel Base
Material Notes: Iron content in composition table calculated as remainder. Ni content includes Co. Nb content include Ta. Tensile and bearing strengths (ultimate and yield) and elongation values reported here are typical for Cold Rolled Sheet, 3 Part Heat Treatment, 0.062 inch (1.57 mm) Thickness samples. Density and magnetic permeability are typical of precipitation hardened INCONEL® alloy 706. Other property values are typical of INCONEL® alloy 706. For optimum creeep and rupture properties, the alloy receives a three part heat treatment as follows: Solution treat 1700-1850°F (925-1010°C) for a time commensurate with section size, then air cool. Stabilizing treatment 1550°F (845°C)/3 hr, air cool. Precipitation treatment 1325°F (720°C)/8 hr, furnace cool at 100°F (55°C)/hr to 1150°F (620°C)/8 hr, air cool. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Ultimate Bearing Strength
- Bearing Yield Strength
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Magnetic Permeability
- Curie Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|