Special Metals MONEL® 404 Copper-Nickel Alloy
Subcategory: Copper Alloy; Nickel Alloy
Material Notes: Copper content in composition table calculated as remainder. Nickel content includes Cobalt. Data provided byCalifornia Fine Wire and the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Magnetic Permeability
- Curie Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Melting Point
|
|
|
|