Special Metals INCOLOY® Alloy 020
Subcategory: Superalloy; Iron Base
Key Words: ASME SB-462 - SB-464, SB-468, Boiler Code Sections III, VIII, IX, UNS N08020; ASTM B 462 - B 464, B 468, B 472 - B 474, B 751
Material Notes: Iron content as remainder; Nb min. is 8xC. A nickel-iron-chromium alloy with additions of copper and molybdenum. It also contains niobium for stabilization against sensitization and resultant intergranular corrosion. The alloy has excellent resistance to general corrosion, pitting, and crevice corrosion in chemicals containing chlorides and sulfuric, phosphoric, and nitric acids. Used for tanks, piping, heat exchangers, pumps, valves, and other process equipment. Standard product forms are round, flats, pipe, tube, plate, sheet, strip, and wire. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|