Special Metals BRIGHTRAY™ Alloy C Electrical Resistance Alloy
Subcategory: Superalloy; Electronic/Magnetic Alloy; Nickel Alloy
Key Words: UNS N06003; ASTM B 344; SAE AMS 5682; DIN 17742; Werkstoff Nr. 2.4869; MIL-C-5031
Material Notes: Nickel content as remainder and includes cobalt. A nickel-chromium electrical-resistance alloy for use at operating temperatures up to 2100°F (1150°C). It contains rare-earth additions for increased oxidation resistance, especially under conditions of frequent switching or wide temperature fluctuations. The alloy has a low temperature coefficient of resistance, making it suitable for control resistors. Used for heating elements in domestic appliances and industrial equipment. The standard product form is wire. Data provided by the manufacturer, Special Metals.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- Specific Heat Capacity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|