Special Metals Shape Memory Alloys Nitinol - Chrome-Doped Superelastic Ni-Ti alloy
Subcategory: Titanium Alloy; Nickel Alloy; Nonferrous Metal
Material Notes: Special Metals Corporation is one of the worlds leading producers of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to the latest medical technology.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Elongation at Yield
- Tensile Set
- Melting Point
- Lower superelastic plateau stress, ksi
- Upper superelastic plateau stress, ksi
|
|
|
|