Industeel CLC 18.10 Ti Ti Stabilized 18Cr-10Ni Austenitic Stainless Steel
Subcategory: Stainless Steel; T S30000 Series Stainless Steel; Metal; Austenitic
Key Words: EURONORM 1.4541 X6CrNiTi 18-10, AFNOR Z6 CNT 18-10, DIN W1.4541, ASTM A 240 – TP 321, UNS S32100
Material Notes: Description: CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This kind of steel is one of the basic grades of the stainless steels range. Titanium bearing (carbide forming element) avoids intergranular corrosion, even on welded pieces without ulterior water quenching. Alloys CLC 18-10Ti exhibit austenitic microstructures free of deleterious carbide precipitations but with CNTi precipitations at the grain boundaries. The grade contains some residual ferrite (~ 4%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenching. The main properties are :- Basic corrosion resistance
- Resistance against intergranular corrosion
- Heat resistant alloy (medium temperature)
- High ductility
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Creep Strength
- Modulus of Elasticity
- Poissons Ratio
- Charpy Impact
- Charpy Impact, Notched Low Temp
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|