Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel

 

Subcategory: Stainless Steel; T S30000 Series Stainless Steel; Metal; Austenitic

Key Words: EURONORM 1.4404 X2CrNiMo 17.12.2, AFNOR Z3 CND 17-11-02, DIN W1.4404, ASTM A 240 TP 316L, UNS S31603

Material Notes:
Description: CLC 17-12-2L is one of the basic grade of the stainless steels range. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform and localized corrosion. Alloy CLC 17-12-2L is an austenitic microstructure grade, free of deleterious carbide precipitations in grain boundaries. The grade contains some residual ferrite (approx. 3%) after solution annealing (1050-1150°C – 1922-2102°F) and water quenching. Chemistry and heat treatments may be optimized in order to control the ferrite content. The CLC 17-2-2L steel resists to wet atmosphere or room temperature solutions containing some chloride or fluoride additions. The steel is not seawater resistant. The alloy may be used in diluted sulphuric acids at low temperature (= 330°C - 626°F) as well as in sour organic solutions. The grade is also well known for its higher ductility, particularly when considering cold forming.

Iron content calculated as remainder.

Information provided by manufacturer.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • Poissons Ratio
  • Charpy Impact
  • Charpy Impact, Notched Low Temp
  • Charpy Impact, Unnotched
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。