Industeel CLC 17.13.5 LN Modified 317LN Mo 4% Austenitic Stainless Steel
Subcategory: Stainless Steel; T S30000 Series Stainless Steel; Metal; Austenitic
Key Words: EURONORM 1.4439 X2CrNiMoN17.13.5, AFNOR Z3CND 18-14 05Az, DIN W 1.4439, ASTM A240 TP 317LNM, UNS S31725, UNS S31726
Material Notes: Description: CLC 17-13-5LN (317LNM) is a Nitrogen alloyed austenitic stainless steel with a high Molybdenum addition (=4%). Alloy CLC 17-13-5LN (317LNM) exhibits austenitic microstructure free of deleterious carbide precipitations in grainboundaries. The grade contains some residual ferrite (=2%) after solution annealing (1100 - 1150°C / 2012 - 2102°F) and water quenching. Its low carbon content avoids the intergranular corrosion, even on welded pieces without an ulterior water quenching. The high Molybdenum content gives this steel a higher resistance to corrosion in chloride containing environments than standard grades (CLC17-12-2L / 316L). Nitrogen additions and a low silicon content have a stabilizing effect on austenitic structure reducing, therefore, precipitation of inter-metallic phases during welding. Nitrogen addition also increases the yield strength compared to CLC 18-15-4L (317L). Its main properties are : high ductility, easy weldability and high corrosion resistance. The main applications are chemical and petrochemical applications, pollution control equipments and chemical tankers.
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|