Industeel CLC 18.15.4L 3% Mo Minimum Austenitic Stainless Steel

 

Subcategory: Stainless Steel; T S30000 Series Stainless Steel; Metal; Austenitic

Key Words: EURONORM 1.4438 X2CrNiMo18.15.4, AFNOR Z3 CND 19-15-04, DIN W 1.4438, ASTM A240 TP 317L, UNS S31703

Material Notes:
Description: CLC 18-15-4L (317L) is an austenitic stainless steel with a 3% minimum Molybdenum addition. Alloys CLC 18-15-4L (317L) exhibit austenitic microstructure free of deleterious carbide precipitations in grain boundaries. The grade contains some residual ferrite (=2%) after solution annealing (1100 - 1150°C/ 2012 - 2102°F) and water quenching. Its low carbon content avoids the intergranular corrosion, even on welded pieces without an ulterior water quenching. The high Molybdenum content gives this steel a higher resistance to corrosion in sulfuric media than standard grades (CLC17-12-2L / 316L). Its main properties are : high ductility, easy weldability and improved corrosion resistance. The main application are chemical tankers, chemical industries and pulp and paper industry.

Iron content calculated as remainder.

Information provided by manufacturer.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。