Industeel CLC 18.15.4L 3% Mo Minimum Austenitic Stainless Steel
Subcategory: Stainless Steel; T S30000 Series Stainless Steel; Metal; Austenitic
Key Words: EURONORM 1.4438 X2CrNiMo18.15.4, AFNOR Z3 CND 19-15-04, DIN W 1.4438, ASTM A240 TP 317L, UNS S31703
Material Notes: Description: CLC 18-15-4L (317L) is an austenitic stainless steel with a 3% minimum Molybdenum addition. Alloys CLC 18-15-4L (317L) exhibit austenitic microstructure free of deleterious carbide precipitations in grain boundaries. The grade contains some residual ferrite (=2%) after solution annealing (1100 - 1150°C/ 2012 - 2102°F) and water quenching. Its low carbon content avoids the intergranular corrosion, even on welded pieces without an ulterior water quenching. The high Molybdenum content gives this steel a higher resistance to corrosion in sulfuric media than standard grades (CLC17-12-2L / 316L). Its main properties are : high ductility, easy weldability and improved corrosion resistance. The main application are chemical tankers, chemical industries and pulp and paper industry.
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|