Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel
Subcategory: Stainless Steel; T S30000 Series Stainless Steel; Metal; Duplex
Key Words: EURONORM 1.4462 - X2 Cr Ni Mo N 22.5.3, AFNOR Z3 CND 22.05.AZ, WERKSTOFF Nr 1.4462, UNS S31803, UNS S32205
Material Notes: Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chromium. This alloy presents higher mechanical and corrosion resistance properties than duplex 22 Cr stainless steels. Its yield strength is about twice that of standard austenitic grades and well in excess of that of nitrogen alloyed austenitics. Operation temperature of UR 45 N+ is generally limited from -50°C to 280°C (- 58°F to 536°F). Lower temperature used particularly for welded structures may also be considered, but needs technical background.
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Poissons Ratio
- Charpy Impact
- Charpy Impact, Notched Low Temp
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|