Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Subcategory: Stainless Steel; T S30000 Series Stainless Steel; Metal; Duplex
Key Words: EN 10088 - EN 10028.7 X2 Cr Ni Mo N 25.6.3 - 1.4410, AFNOR Z3 CND 25.07 AZ, ASTM A 240 - UNS S32750, SAF 2507
Material Notes: Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to reduce weight. The molybdenum and nitrogen additions have been optimized in order to obtain the best corrosion resistance properties even for heavy plates. Its high nitrogen content improves the structure stability particularly in HAZ. The CLI - SAF 2507® (URANUS® 47N+) grade is an overalloyed variant of the former UR 47N grade of CLI. CLI - SAF 2507® has improved corrosion resistance properties when compared to duplex 2205 type materials, or even to URANUS® 47N. It is designed for service in severe corrosive conditions. The alloy is particularly resistant to stress corrosion cracking and crevice corrosion. CLI - SAF 2507® is a cost efficient grade designed for Oil & Gas industry, Seawater applications, Desalination plants, Geothermal wells or Refineries and Petrochemical plants.
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Density
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Poissons Ratio
- Charpy Impact
- Charpy Impact, Notched Low Temp
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|