Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Subcategory: Stainless Steel; T S30000 Series Stainless Steel; Metal; Duplex
Key Words: EURONORM 1. 4507 - X2 Cr Ni Mo Cu N 25.6.3, AFNOR Z3 CNDU 25.07 AZ, UNS S32550, UNS S32520
Material Notes: Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to reduce weight. The molybdenum and nitrogen additions have been optimized in order to obtain the best corrosion resistance properties even for heavy plates. High nitrogen content improves the structure stability particularly in HAZ. Its corrosion resistance is much better than UR B6/N08904 and roughly equivalent to 6 Mo super austenitic alloys. Copper additions increase the corrosion resistance properties, particularly in sulfuric acid media. URANUS® 52N+ is a cost efficient grade designed for offshore, marine, phosphoric acid, sulfuric acid applications... as well as pollution control equipments.
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Density
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Poissons Ratio
- Charpy Impact
- Charpy Impact, Notched Low Temp
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|