Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal; Austenitic
Key Words: EN 10095 X8 Cr Ni 25-21 - 1.4845, EN 10028-7 X6 Cr Ni 25-20, AFNOR Z8 CN 25.20, DIN W. Nr 1.4845, ASTM Type 310S
Material Notes: Description: CLI SIRIUS 310 grade is a fully austenitic stainless steel containing 25% Cr, 0.6% Si and 20% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resistance behavior. Carbon additions are optimized in order to provide improved creep resistance properties. Alloy CLI SIRIUS 310 can be easily welded. The alloy is designed for high temperature applications up to 1100°C (2012°F) in oxidizing atmospheres. The alloy can be also used in slightly oxidizing atmospheres,, nitriding, cementing, sulphurising conditions as well as with thermal cyclings, but the maximum temperature of use will be reduced.
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Creep Strength
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|